Skip to main page content
U.S. flag

An official website of the United States government

Dot gov

The .gov means it’s official.
Federal government websites often end in .gov or .mil. Before sharing sensitive information, make sure you’re on a federal government site.

Https

The site is secure.
The https:// ensures that you are connecting to the official website and that any information you provide is encrypted and transmitted securely.

Access keys NCBI Homepage MyNCBI Homepage Main Content Main Navigation

Search Page

Filters

My NCBI Filters

Results by year

Table representation of search results timeline featuring number of search results per year.

Year Number of Results
1988 1
1989 17
1990 10
1991 14
1992 18
1993 10
1994 11
1995 6
1996 5
1997 4
1998 2
1999 4
2000 3
2001 4
2003 3
2005 2
2006 1
2007 1
2008 1
2009 2
2011 1
2012 2
2013 1
2014 3
2017 1
2018 1
2021 1
2024 0

Text availability

Article attribute

Article type

Publication date

Search Results

127 results

Results by year

Filters applied: . Clear all
Page 1
Laboratory strength of glass ionomer and zinc phosphate cements.
Piwowarczyk A, Ottl P, Lauer HC. Piwowarczyk A, et al. J Prosthodont. 2001 Sep;10(3):140-7. doi: 10.1111/j.1532-849x.2001.00140.x. J Prosthodont. 2001. PMID: 11641841
MATERIALS AND METHODS: The examined materials were 2 cermet cements (Ketac Silver [ESPE, Seefeld, Germany] and Chelon Silver [ESPE]), 1 metal-reinforced glass ionomer cement (Miracle Mix [GC Dental Industrial Corp, Tokyo, Japan]), 2 conventional glass ionomer cements (Ketac
MATERIALS AND METHODS: The examined materials were 2 cermet cements (Ketac Silver [ESPE, Seefeld, Germany] and Chelon Silver [ESPE]), 1 meta …
Oral Function Improves Interfacial Integrity and Sealing Ability Between Conventional Glass Ionomer Cements and Dentin.
Toledano M, Osorio R, Cabello I, Osorio E, Toledano-Osorio M, Aguilera FS. Toledano M, et al. Microsc Microanal. 2017 Feb;23(1):131-144. doi: 10.1017/S1431927617000010. Epub 2017 Feb 2. Microsc Microanal. 2017. PMID: 28148310 Free article.
The unloaded specimens of sound and carious dentin were deficiently hybridized when Ketac Bond was used. Ketac Bond samples showed an absorption layer and an adhesive layer that were scarcely affected by fluorescein penetration (nanoleakage), in sound …
The unloaded specimens of sound and carious dentin were deficiently hybridized when Ketac Bond was used. Ketac Bond
Bonding glass-ionomer cements to chemomechanically-prepared dentin.
McInnes-Ledoux PM, Weinberg R, Grogono A. McInnes-Ledoux PM, et al. Dent Mater. 1989 May;5(3):189-93. doi: 10.1016/0109-5641(89)90012-2. Dent Mater. 1989. PMID: 2700179 Clinical Trial.
The remaining dentin in 30 of the teeth prepared with the chemomechanical technique, and in all of the teeth prepared with mechanical drilling, was treated with 10% aqueous polyacrylic acid for 10 seconds. Groups of 15 teeth were assigned for bonding with either Ketac-B
The remaining dentin in 30 of the teeth prepared with the chemomechanical technique, and in all of the teeth prepared with mechanical drilli …
The effect of different liners on the bond strength of a compomer to primary teeth dentine: in vitro study.
Frankenberger R, Nassiri S, Lücker S, Lygidakis NN, Krämer N. Frankenberger R, et al. Eur Arch Paediatr Dent. 2021 Aug;22(4):643-649. doi: 10.1007/s40368-020-00601-2. Epub 2021 Feb 3. Eur Arch Paediatr Dent. 2021. PMID: 33537902
Six test groups were centrally covered with different protective liners/base materials: Kerr Life (KL), IRM zinc oxide eugenol cement (IRM), Ketac Bond (KB), Vitrebond (VB), Dycal (DY), and mineral trioxide aggregate (MTA). ...
Six test groups were centrally covered with different protective liners/base materials: Kerr Life (KL), IRM zinc oxide eugenol cement (IRM), …
Retention and caries prevention of Vitremer and Ketac-bond used as occlusal sealants.
Pereira AC, Basting RT, Pinelli C, de Castro Meneghim M, Werner CW. Pereira AC, et al. Am J Dent. 1999 Apr;12(2):62-4. Am J Dent. 1999. PMID: 10477984 Clinical Trial.
They were divided into three groups: (a) control group (n = 432 teeth); (b) Vitremer experimental group (n = 200 teeth), and (c) Ketac-Bond experimental group (n = 200 teeth). In the experimental groups, Vitremer was applied on teeth 16 and 46 whereas Ketac- …
They were divided into three groups: (a) control group (n = 432 teeth); (b) Vitremer experimental group (n = 200 teeth), and (c) Ketac
Evaluation of shear bond strength of silorane resin to conventional, resin-modified glass ionomers and nano-ionomer cements.
Babannavar R, Shenoy A. Babannavar R, et al. J Investig Clin Dent. 2014 Nov;5(4):295-300. doi: 10.1111/jicd.12024. Epub 2013 Jan 25. J Investig Clin Dent. 2014. PMID: 23355365
MATERIALS AND METHODS: Shear bond strengths of Vitrebond (Group I), Ketac N100 (Group II) and Ketac Bond (Group III) glass ionomer cements to the composite Filtek P90 were evaluated. ...Vitrebond) appears to be preferable to nano-ionomer glass ionomer cement (i.e. K …
MATERIALS AND METHODS: Shear bond strengths of Vitrebond (Group I), Ketac N100 (Group II) and Ketac Bond (Group III) glass ion …
Microleakage of endodontic access cavities restored with composites.
Barkhordar RA, Kempler D. Barkhordar RA, et al. J Calif Dent Assoc. 1997 Mar;25(3):215-8. J Calif Dent Assoc. 1997. PMID: 9452662
The endodontic access cavities were later treated by Scotchbond Multipurpose, All-Bond 2, Vitrebond and Ketac-Bond. Half the access cavities within each group were filled by Coltene Microhybrid H.P., a chemically cured microhybrid composite. ...As for the dentin pre …
The endodontic access cavities were later treated by Scotchbond Multipurpose, All-Bond 2, Vitrebond and Ketac-Bond. Half the a …
Mechanical properties and microstructures of glass-ionomer cements.
Xie D, Brantley WA, Culbertson BM, Wang G. Xie D, et al. Dent Mater. 2000 Mar;16(2):129-38. doi: 10.1016/s0109-5641(99)00093-7. Dent Mater. 2000. PMID: 11203534
Vitremer (3M) had the highest values of FS and DTS; Fuji II LC (GC International) and Ketac-Molar (ESPE) had the highest CS; Ketac-Fil (ESPE) had the highest KHN. Ketac-Bond (ESPE) had the lowest FS; alpha-Silver (DMG-Hamburg) had the lowest CS. Four GICs (alpha-Fil …
Vitremer (3M) had the highest values of FS and DTS; Fuji II LC (GC International) and Ketac-Molar (ESPE) had the highest CS; Ketac-Fil (ESPE …
In vitro mechanical stimulation facilitates stress dissipation and sealing ability at the conventional glass ionomer cement-dentin interface.
Toledano M, Osorio R, Osorio E, Cabello I, Toledano-Osorio M, Aguilera FS. Toledano M, et al. J Dent. 2018 Jun;73:61-69. doi: 10.1016/j.jdent.2018.04.006. Epub 2018 Apr 10. J Dent. 2018. PMID: 29653140
OBJECTIVE: The aim of this study was to evaluate the induced changes in the chemical and mechanical performance at the glass-ionomer cement-dentin interface after mechanical load application. METHODS: A conventional glass-ionomer cement (GIC) (Ketac Bond), and a res …
OBJECTIVE: The aim of this study was to evaluate the induced changes in the chemical and mechanical performance at the glass-ionomer cement- …
Bond strength of glass-ionomer cement and composite resin combinations.
Oilo G, Um CM. Oilo G, et al. Quintessence Int. 1992 Sep;23(9):633-9. Quintessence Int. 1992. PMID: 1287716
The tensile bond strength to dentin was measured for three glass-ionomer cement and composite resin combinations: two light-curing glass-ionomer cements (Vitrebond and XR-Ionomer) and one traditional glass-ionomer cement (Ketac-Bond), two adhesive systems (Scotchbon …
The tensile bond strength to dentin was measured for three glass-ionomer cement and composite resin combinations: two light-curing glass-ion …