Wet-spinning of regenerated silk fiber from aqueous silk fibroin solution: discussion of spinning parameters.

Author information

1
The Key Laboratory of Molecular Engineering of Polymers of MOE, Department of Macromolecular Science, Laboratory of Advanced Materials, Fudan University, Shanghai 200433, People's Republic of China.

Abstract

Regenerated silk fibroin (RSF) fibers were obtained by extruding a concentrated aqueous silk fibroin solution into an ammonium sulfate coagulation bath. A custom-made simplified industrial-type wet-spinning device with continuous mechanical postdraw was used. The effect of dope concentration, coagulation bath, extrusion rate, and postdraw treatment on the morphology of RSF fiber was examined. The results showed that although RSF fiber could be formed with dope concentration between 13 and 19% (w/w), the ones spun from 15% RSF solution showed the most regular morphology being dense and homogeneous in cross-section with a smooth surface and a uniform cylindrical shape. Though it had little effect on morphology, postdraw treatment especially under steam, significantly improved the mechanical properties of the RSF fibers.

PMID:
19860400
DOI:
10.1021/bm900840h
[Indexed for MEDLINE]
PubMed Commons home

PubMed Commons

0 comments
How to join PubMed Commons

    Supplemental Content

    Full text links

    Icon for American Chemical Society
    Loading ...
    Support Center