Microshear bond strength of preheated silorane- and methacrylate-based composite resins to dentin

Scanning. 2016 Jan-Feb;38(1):63-9. doi: 10.1002/sca.21242. Epub 2015 Sep 18.

Abstract

The aim of this study was to investigate the effect of preheating on microshear bond strength (MSBS) of silorane and methacrylate-based composite resins to human dentin. The teeth were randomly divided into three main groups: (1) composite resins were heated upto 68 °C; (2) cooled to 4 °C; and (3) control [room temperature (RT)]. Each group was then randomly subdivided into four subgroups according to adhesive system used [Solobond M (Voco), All Bond SE (Bisco), Clearfil SE Bond (CSE) (Kuraray), Silorane adhesive system (SAS) (3M ESPE)]. Resin composite cylinders were formed (0.9 mm diameter × 0.7 mm length) and MSBS of each specimen was tested. The preheated groups exhibited the highest MSBS (p < 0.001) and the groups cooled to 4 °C exhibited the lowest MSBS (p < 0.001). The CSE showed higher MSBS than the other adhesives (p < 0.001). This study concludes that preheating of composite resins may be an alternative way to increase the MSBS of composites on dentin.

Keywords: dentin; microshear bond strength; preheating; silorane-based composite resin.

MeSH terms

  • Composite Resins / pharmacology*
  • Composite Resins / radiation effects
  • Dentin / metabolism*
  • Hot Temperature*
  • Humans
  • Mechanical Phenomena*
  • Methacrylates / pharmacology*
  • Methacrylates / radiation effects
  • Silorane Resins / pharmacology*
  • Silorane Resins / radiation effects
  • Treatment Outcome

Substances

  • Composite Resins
  • Methacrylates
  • Silorane Resins