    Proc Finn Dent Soc. 1992;88 Suppl 1:225-42.

    Smear layer--materials surface.

    Source

    Department of Oral Biology, School of Dentistry, University of Missouri-Kansas City.

    Abstract

    SEM and TEM photomicrographs were presented of the smear layer and several dentin-adhesive interfaces. It was shown that as the wetting and penetration of the dentin adhesive increased, the shear bond strength also increased. Three categories of dentin adhesives were presented. Category one included Scotchbond, Dentin Adhesit and Gluma, with shear bond strength values between 5 and 7 MPa; the second category, dentin adhesives based on Dr. Bowen's research, included Tenure and Mirage Bond, with shear bond strengths between 8 and 14 MPa; the third category included Superbond and Scotchbond 2, with shear bond strength values up to 20 MPa. Failures occurred at the interface or in the resin adhesive for materials in categories one and two; failures occurred through the dentin or composite for materials in category three.

    PMID:
    1508878
    [PubMed - indexed for MEDLINE]

      Supplemental Content

      Save items

      loading

      Recent activity

      Your browsing activity is empty.

      Activity recording is turned off.

      Turn recording back on

      See more...
      Write to the Help Desk